| Magnetization Direction | Axial | 
|---|---|
| Tolerance | +/- 0.05 Mm | 
| Standard | ISO9001/ROHS/ | 
| Package Size | 340mm×255mm×75mm | 
| Density | 4.9 G/cm3 | 
| Curie Temperature | 450°C | 
|---|---|
| Competitive Advantage | High Temperature Resistance | 
| Density | 4.9 G/cm3 | 
| Magnetization Direction | Axial | 
| Size | (R51.8mm-r43.1mm)×39.0mm | 
| Type | Permanent | 
|---|---|
| Origin | Sichuan, China (Mainland), | 
| Intrinsic Coercivity | 240-280 KA/m | 
| Curie Temperature | 450°C | 
| Coercivity | 235-275 KA/m | 
| Origin | Sichuan, China (Mainland), | 
|---|---|
| Intrinsic Coercivity | 240-280 KA/m | 
| Standard | ISO9001/ROHS/ | 
| Magnetic Energy Product | 27-30 KJ/m3 | 
| Application | Motors, Speakers, Magnetic Separators | 
| Intrinsic Coercivity | 240-280 KA/m | 
|---|---|
| Magnetization Direction | Axial | 
| Tolerance | +/- 0.05 Mm | 
| Origin | Sichuan, China (Mainland), | 
| Package Size | 340mm×255mm×75mm | 
| Size | (R51.8mm-r43.1mm)×39.0mm | 
|---|---|
| Type | Permanent | 
| Package Size | 340mm×255mm×75mm | 
| Competitive Advantage | High Temperature Resistance | 
| Coercivity | 235-275 KA/m | 
| Standard | ISO9001/ROHS/ | 
|---|---|
| Coercivity | 235-275 KA/m | 
| Density | 4.9 G/cm3 | 
| Curie Temperature | 450°C | 
| Intrinsic Coercivity | 240-280 KA/m |